LCD glass waste weak alkali activation
a. b. c. Figure a. Opal glass with coarse LCD loading dried at 40°C for 7 days. Figure b. LCD glass activated with KOH after curing at 40°C for 7 days and firing at 900°C. Figure c. LCD glass foam activated with NaOH after curing and firing at 900°C. The LCD glass waste was ground…
Read more